ALU INVEST for casting metal 1 kg

ALU INVEST for casting metal 1 kg

ALU INVEST Ceramic mold making powder used for casting aluminium and bronze
Price with VAT:
5,86 €
ADD TO CART

 

ADVANTAGES 

- smooth-walled casts

-fast curing

-simple demolding

-used for casting in cuvettes up to 1000 kg

-used for casting bronze and alluminium

 

MIXING RATIO

Powder : Water   1 kg : 0,36/,40 ltr

Mixture volume:  0,77 - 0,79 ltr

Pot life: approx. 20 minutes

Curing time before heating: min. 90 minutes

Heating regime: table 1 and table 2

 

USAGE

- powder and water temperature 20-23°C

- water temperature over 30-35°C shortens the curing time, lower temperatures elongate it

- mixing ratio may variate within the prescribed ratio according to the shape's complexity

- Pour the powder in the water, stir thoroughly, taking care not to mix in too much air (air bubbles may form)
- Vacuum the mixture if possible
- cure at room temperature for at least 90 minutes before heating
- Evaporate the wax – heat for at least 1,5 hours
- Insert into a cold furnace or a furnace preheated  to 150-180°C
- Demold after cooling to room temperature

 

 

Related products

    Samson Kamnik d.o.o., Kovinarska cesta 28 1241 Kamnik T: +38 1 8317 255; +386 1 8319 260, F: +386 1 8317 179 E: splet@samson-kamnik.si
    Cookie - Analitics
    They are used to record the website's obscurity analysis and provide us with data to provide a better user experience.
    Cookie - social
    Cookies required for plug-ins for sharing content from social media sites.
    Cookie - chat
    Cookies allow you to sign up, contact and communicate through the communication plug-in on the page.
    Cookie - marketing
    They target targeted advertising based on past user's activity on other sites.
    What are cookies?
    By visiting and using the site, you consent to the use and recording of cookies.OK Learn more about cookies